Mahalo iā ʻoe no ke kipa ʻana i nā mea kikoʻī scatter glassfiber cabron fiber.Ke hoʻohana nei ʻoe i kahi polokalamu kele pūnaewele me ke kākoʻo CSS palena ʻole.No ka ʻike maikaʻi loa, manaʻo mākou e hoʻohana i kahi polokalamu kele pūnaewele hou (a i ʻole e hoʻopau i ke ʻano Compatibility Mode ma Internet Explorer).Eia kekahi, e hōʻoia i ke kākoʻo mau, hōʻike mākou i ka pūnaewele me ka ʻole o nā styles a me JavaScript.
Manaʻo ʻia ʻo Polymer-reinforced concrete (FRP) he ʻano hana hou a hoʻokele waiwai no ka hoʻoponopono ʻana i ka hale.Ma kēia noiʻi ʻana, ua koho ʻia ʻelua mau mea maʻamau [carbon fiber reinforced polymer (CFRP) a me glass fiber reinforced polymer (GFRP)] no ke aʻo ʻana i ka hopena hoʻoikaika ʻana o ke kaʻa ma nā wahi paʻakikī.Kūkākūkā ʻia ke kūʻē ʻana o ke kōkō i loaʻa i ka FRP i ka hoʻouka ʻana i ka sulphate a me nā pōʻai manuahi e pili ana.Electron microscopy no ke aʻo ʻana i ka ʻili a me ka hoʻohaʻahaʻa ʻana o loko o ka ʻiʻo i ka wā e hoʻoneʻe ʻia ai.Ua kālailai ʻia ke degere a me ka hana o ka sodium sulfate corrosion e ka pH waiwai, SEM electron microscopy, a me EMF ikehu spectrum.Ua hoʻohana ʻia nā hoʻāʻo ikaika compressive Axial no ka loiloi i ka hoʻoikaika ʻana o nā kolamu koʻikoʻi FRP-constrained, a ua loaʻa nā pilina koʻikoʻi-koʻikoʻi no nā ʻano like ʻole o ka paʻa ʻana o FRP i kahi kaiapuni i hui ʻia erosive.Ua hana ʻia ka loiloi hewa e calibrate i nā hopena hoʻokolohua me ka hoʻohana ʻana i ʻehā mau hiʻohiʻona wānana.Hōʻike nā ʻike a pau he paʻakikī a paʻakikī ke kaʻina hana hoʻohaʻahaʻa o ka ʻuala i kaupalena ʻia FRP ma lalo o nā koʻikoʻi conjugate.Hoʻonui mua ka sodium sulfate i ka ikaika o ke konima ma kona ʻano maka.Eia nō naʻe, hiki i nā pōʻai maloʻo hoʻoheheʻe ma hope ke hoʻonui i ka haki ʻana o ka ʻiʻo, a ʻo ka sodium sulfate e hoʻemi hou i ka ikaika o ke kaʻa ma o ka paipai ʻana i ka māhā.Manaʻo ʻia kahi kŘkohu helu pololei e hoʻohālikelike i ka pilina koʻikoʻi-koʻikoʻi, he mea koʻikoʻi no ka hoʻolālā ʻana a me ka loiloi ʻana i ke ola pōʻaiapuni o ke koʻo FRP-constrained.
Ma ke ʻano he ʻano hoʻoikaika paʻa paʻa hou i noiʻi ʻia mai ka makahiki 1970, loaʻa iā FRP nā pōmaikaʻi o ke kaumaha māmā, ka ikaika kiʻekiʻe, ka pale ʻana i ka corrosion, ke kūpaʻa luhi a me ke kūkulu kūpono ʻana1,2,3.Ke emi nei nā kumukūʻai, ua lilo ia i mea maʻamau i nā noi ʻenekinia e like me fiberglass (GFRP), carbon fiber (CFRP), basalt fiber (BFRP), a me aramid fiber (AFRP), ʻo ia ka FRP maʻamau i hoʻohana ʻia no ka hoʻoikaika ʻana i ka hale4, 5 Hiki ke ho'omaika'i i ke ka'ina hana pa'a a pale i ka hā'ule mua.Eia nō naʻe, pili pinepine nā kaiapuni o waho i ka ʻenekinia mechanical i ka lōʻihi o ka FRP-limited concrete, e hōʻemi ana i kona ikaika.
Ua aʻo kekahi mau mea noiʻi i ke koʻikoʻi a me ka hoʻololi ʻana i ke koʻikoʻi me nā ʻano like ʻole a me nā nui.ʻO Yang et al.Ua ʻike ʻo 6 i ka hoʻopili maikaʻi ʻana o ke koʻikoʻi a me ke koʻikoʻi me ka ulu ʻana o ka mānoanoa fibrous tissue.Ua loaʻa ʻo Wu et al.7 i nā pihi koʻikoʻi-koʻikoʻi no ka FRP-constrained concrete me ka hoʻohana ʻana i nā ʻano fiber like ʻole e wānana i nā koʻikoʻi a me nā ukana hope loa.Ua ʻike ʻo Lin et al.8 he ʻokoʻa loa nā hiʻohiʻona FRP stress-strain no ka poepoe, square, rectangular, a me elliptical bars, a ua hoʻomohala i kahi hoʻolālā hoʻolālā hoʻoluhi koʻikoʻi me ka hoʻohana ʻana i ka lākiō o ka laulā a me ka radius kihi e like me nā ʻāpana.Ua ʻike ʻo Lam et al.9 ʻo ka overlap like ʻole a me ka curvature o ka FRP i hopena i ka liʻiliʻi o ka haʻihaʻi a me ke koʻikoʻi i ka FRP ma mua o nā hoʻāʻo tensile slab.Eia hou, ua aʻo nā kānaka ʻepekema i nā kaohi hapa a me nā ʻano kaohi hou e like me nā pono hoʻolālā honua maoli.ʻO Wang et al.[10] hana i nā ho'āʻo hoʻopaʻapaʻa axial ma ka piha, hapa a me ka paʻa ʻole ʻia i loko o ʻekolu mau ʻano palena.Ua hoʻomohala ʻia kahi ʻano hoʻohālike "stress-strain" a ua hāʻawi ʻia nā coefficient o ka hopena palena no ka ʻāpana i pani ʻia.ʻO Wu et al.Ua hoʻomohala ʻo 11 i kahi ala no ka wānana ʻana i ke koʻikoʻi-koʻikoʻi hilinaʻi o FRP-constrained concrete e nānā i nā hopena nui.Moran et al.12 loiloi i ka axial monotonic compression waiwai o ka constrained concrete me FRP helical strips a loaa kona stress-strain curves.Eia naʻe, ʻo ka haʻawina ma luna nei e nānā nui i ka ʻokoʻa ma waena o ka ʻāpana paʻa a me ka paʻa paʻa piha.ʻAʻole i aʻo nui ʻia ke kuleana o nā FRP e kaupalena ana i nā ʻāpana koneki.
Eia hou, ua loiloi ka haʻawina i ka hana o ka FRP-palena ʻia ma ke ʻano o ka ikaika compressive, ka hoʻololi ʻana, ka modulus mua o ka elasticity, a me ka modulus paʻakikī paʻakikī ma lalo o nā kūlana like ʻole.ʻO Tijani et al.Ua ʻike ʻo 13,14 i ka emi ʻana o ka hiki ke hoʻoponopono ʻia ʻo FRP-palena ʻia me ka piʻi ʻana o ka pōʻino i nā hoʻokolohua hoʻoponopono FRP ma ka pā i hoʻopōʻino mua ʻia.Ma et al.[15] ua aʻo i ka hopena o ka pōʻino mua ma nā kolamu koʻa i hoʻopaʻa ʻia ʻo FRP a manaʻo ʻia he mea ʻole ka hopena o ka degere poino i ka ikaika tensile, akā he hopena koʻikoʻi i nā deformations ʻaoʻao a me ka longitudinal.Eia naʻe, ʻo Cao et al.16 nānā 'ana i nā pihi ko'iko'i-ko'iko'i a me nā pō'ino enveloppe ko'iko'i o FRP i ho'opilikia 'ia e ka poino mua.Ma waho aʻe o nā haʻawina e pili ana i ka hāʻule ʻana o ke kōkō mua, ua mālama ʻia kekahi mau haʻawina e pili ana i ka lōʻihi o ka paʻa paʻa FRP ma lalo o nā kūlana kūlohelohe.Ua aʻo kēia poʻe ʻepekema i ka hoʻohaʻahaʻa ʻia ʻana o ke koki i kaupalena ʻia e FRP ma lalo o nā kūlana paʻakikī a hoʻohana i nā ʻenehana loiloi pōʻino e hana i nā kumu hoʻohālike e wānana i ke ola lawelawe.Xie et al.17 ua hoʻokomo ʻo FRP-constrained concrete i loko o ka hydrothermal environment a ua ʻike ʻo ia ua hoʻopilikia nui nā kūlana hydrothermal i nā waiwai mechanical o FRP, e hopena i ka emi mālie o kona ikaika compressive.I loko o kahi ʻakika-base, e hoʻohaʻahaʻa ʻia ka pilina ma waena o CFRP a me ke kaʻa.E like me ka piʻi ʻana o ka manawa immersion, e emi nui ana ka nui o ka hoʻokuʻu ʻana i ka ikehu o ka luku ʻana i ka papa CFRP, ka mea e alakaʻi i ka luku ʻana i nā samples interfacial18,19,20.Eia hou, ua aʻo kekahi poʻe ʻepekema i ka hopena o ka hoʻoheheʻe ʻana a me ka hoʻoheheʻe ʻana i ka ʻuala FRP-limited.Ua ʻike ʻo Liu et al.21 he lōʻihi ka lōʻihi o ka CFRP rebar ma lalo o nā pōʻai hau hau ma muli o ka modulus dynamic pili, ka ikaika compressive, a me ka ratio stress-strain.Eia kekahi, ua hoʻolālā ʻia kahi hiʻohiʻona e pili ana i ka hoʻohaʻahaʻa ʻana i nā ʻano mechanical o ke koneki.Eia naʻe, ua helu ʻo Peng et al.22 i ke ola o ka CFRP a me nā mea hoʻopili paʻa me ka hoʻohana ʻana i ka ʻikepili pōʻai wela a me ka hau.ʻO Guang et al.Ua hana ʻo 23 i nā hoʻāʻo hoʻoheheʻe wikiwiki ʻana o ka ʻiʻo a manaʻo ʻia kahi ala no ka loiloi ʻana i ke kū ʻana o ka hau ma muli o ka mānoanoa o ka papa i poino ma lalo o ka hoʻolaha ʻana i ka hau.ʻO Yazdani et al.Ua aʻo ʻo 24 i ka hopena o nā papa FRP i ke komo ʻana o nā ion chloride i loko o ke kaʻa.Hōʻike nā hopena i ka pale kemika o ka papa FRP a hoʻokaʻawale i ka ʻāpana o loko mai nā ion chloride waho.Liu et al.25 simulated peel ho'āʻo kūlana no ka sulfate-corroded FRP kaila, hana i ka pahee kükohu, a wanana degradation o ka FRP-paʻa interface.ʻO Wang et al.Ua hoʻokumu ʻo 26 i kahi kumu hoʻohālike koʻikoʻi no ka FRP-constrained sulphate-eroded concrete ma o nā hoʻokolohua uniaxial compression.ʻO Zhou et al.[27] ua aʻo i ka pōʻino o ka paʻakai paʻa ʻole i hoʻokumu ʻia e ka hui ʻana o ka paʻakai paʻakai a no ka manawa mua i hoʻohana i kahi hana logistic e wehewehe i ke ʻano hana hāʻule.Ua holomua nui kēia mau haʻawina i ka loiloi ʻana i ka lōʻihi o ke koki palena FRP.Eia nō naʻe, ʻo ka hapa nui o ka poʻe noiʻi i kālele i ka hoʻohālike ʻana i ka media erosive ma lalo o kahi kūlana maikaʻi ʻole.E pōʻino pinepine ʻia ka palaki ma muli o ka hili ʻia ʻana e nā ʻano ʻano kaiapuni.ʻO kēia mau kūlana kaiapuni i hui pū ʻia e hoʻohaʻahaʻa loa i ka hana ʻana o ke koki i kaupalena ʻia FRP.
ʻO nā pōʻai Sulfation a me ka hoʻoheheʻe ʻana he ʻelua mau ʻāpana koʻikoʻi e pili ana i ka lōʻihi o ke kaʻa.Hiki i ka ʻenehana localization FRP ke hoʻomaikaʻi i nā waiwai o ke kaʻa.Hoʻohana nui ʻia ia i ka ʻenekinia a me ka noiʻi, akā i kēia manawa aia kona mau palena.Ua hoʻopaʻa ʻia kekahi mau haʻawina i ke kūʻē ʻana o ke koki i hoʻopaʻa ʻia ʻo FRP i ka palaka sulfate ma nā wahi anu.ʻO ke kaʻina hana o ka hoʻoheheʻe ʻia ʻana o ka paʻa paʻa paʻa, semi-paʻa a wehe ʻia e ka sodium sulfate a me ka freeze-thaw e pono e noiʻi hou ʻia, ʻoi aku ka nui o ke ʻano semi-paʻa hou i wehewehe ʻia ma kēia ʻatikala.Ua aʻo pū ʻia ka hopena hoʻoikaika i nā kolamu koneki ma ka hoʻololi ʻana i ke kauoha o ka paʻa ʻana o FRP a me ka erosion.Hoʻololi ʻia ka microcosmic a me ka macroscopic i ka hāpana i hoʻokumu ʻia e ka erosion bond e ka microscope electron, pH test, SEM electron microscope, EMF energy spectrum analysis and uniaxial mechanical test.Eia kekahi, ke kūkākūkā nei kēia haʻawina i nā kānāwai e pili ana i ka pilina koʻikoʻi-koʻikoʻi i hana ʻia ma ka hoʻāʻo ʻana i ka mechanical uniaxial.Ua hōʻoia ʻia ka hoʻokolohua hoʻāʻo ʻia i nā koʻikoʻi koʻikoʻi a me nā koina koʻikoʻi e ka nānā ʻana i nā hewa me ka hoʻohana ʻana i ʻehā mau hiʻohiʻona koʻikoʻi.Hiki i ke kŘkohu i manaʻo ʻia ke wānana piha i ke koʻikoʻi a me ka ikaika o ka mea, pono ia no ka hana hoʻoikaika FRP e hiki mai ana.ʻO ka mea hope loa, ʻo ia ke kumu noʻonoʻo no ka manaʻo kūpaʻa paʻakai paʻakai FRP.
Ke loiloi nei kēia noiʻi ʻana i ka pōʻino o ke koki palena FRP me ka hoʻohana ʻana i ka corrosion solution sulfate i hui pū ʻia me nā pōʻai manuahi.Ua hōʻike ʻia nā loli microscopic a me ka macroscopic i hoʻokumu ʻia e ka erosion concrete me ka hoʻohana ʻana i ka microscopy electron scanning, ka hoʻāʻo pH, ka spectroscopy ikehu EDS, a me ka hoʻāʻo uniaxial mechanical.Eia hou, ua noiʻi ʻia nā ʻano mechanical a me nā hoʻololi koʻikoʻi-koʻikoʻi o FRP-constrained concrete i hoʻopaʻa ʻia me ka hoʻohana ʻana i nā hoʻokolohua axial compression.
Loaʻa ka FRP Confined Concrete me ka ʻōpala maka, ka mea hoʻopili waho FRP a me ka epoxy adhesive.Ua kohoʻiaʻelua mau mea hoʻoheheʻe waho: CFRP a me GRP, nā waiwai o nā mea i hōʻikeʻia ma ka Papa 1. Ua hoʻohanaʻia nā epoxy resins A a me B e like me nā mea hoʻopili (mixing ratio 2: 1 ma ka leo).Laiki.Hōʻike ka 1 i nā kikoʻī o ke kūkulu ʻana i nā mea hoʻohui ʻia.Ma ke Kiʻi 1a, ua hoʻohana ʻia ʻo Swan PO 42.5 Portland cement.ʻO nā mea hōʻiliʻili nui he pōhaku basalt me ke anawaena o 5-10 a me 10-19 mm, e like me ka mea i hōʻike ʻia ma ka fig.1b a me c.Ma ke ʻano he hoʻopiha maikaʻi ma Fig. 1g i hoʻohana i ke one kahawai maoli me ka modulus fineness o 2.3.E hoʻomākaukau i kahi hopena o ka sodium sulfate mai nā granule o ka sodium sulfate anhydrous a me kahi nui o ka wai.
ʻO ka hui ʻana o ka hui ʻana: a - cement, b - aggregate 5-10 mm, c - aggregate 10-19 mm, d - one kahawai.
ʻO 30 MPa ka ikaika o ka hoʻolālā ʻana, kahi e loaʻa ai kahi hoʻonohonoho sima hou o 40 a 100 mm.Hōʻike ʻia ka lākiō hui ʻia ma ka Papa 2, a ʻo ka lakio o ka coarse aggregate 5-10 mm a me 10-20 mm he 3:7.Ua hoʻohālike ʻia ka hopena o ka launa pū ʻana me ke kaiapuni ma o ka hoʻomākaukau mua ʻana i kahi solution 10% NaSO4 a laila ninini i ka hopena i loko o kahi keʻena pōʻaiapuni freeze-thaw.
Ua hoʻomākaukau ʻia nā huila paʻa i loko o kahi hui pū ʻia 0.5 m3 a ua hoʻohana ʻia ka pūʻulu holoʻokoʻa no ka waiho ʻana i nā laʻana i koi ʻia.ʻO ka mea mua, ua hoʻomākaukau ʻia nā mea hana e like me ka Papa 2, a ua hoʻohui ʻia ka sima, ke one a me ka coarse aggregate no ʻekolu mau minuke.A laila e māhele like i ka wai a hoʻoulu no 5 mau minuke.A laila, hoʻolei ʻia nā laʻana paʻa i loko o nā mole cylindrical a hoʻopaʻa ʻia ma luna o kahi pākaukau haʻalulu (ʻo ke anawaena 10 knm, ke kiʻekiʻe 20 knm).
Ma hope o ka ho'ōla ʻana no nā lā 28, ua wahī ʻia nā laʻana me ka mea FRP.Kūkākūkā kēia haʻawina i ʻekolu mau ʻano no nā kolamu i hoʻopaʻa ʻia, me ka paʻa piha, semi-constrained, a me ka palena ʻole.ʻElua ʻano, CFRP a me GFRP, hoʻohana ʻia no nā mea liʻiliʻi.FRP Paʻa piha ʻia ʻo FRP pūpū, 20 knm ke kiʻekiʻe a 39 knm ka lōʻihi.ʻAʻole i hoʻopaʻa ʻia me ka epoxy ka luna a me ka lalo o ka pahu paʻa FRP.ʻO ke kaʻina hana hoʻāʻo semi-hermetic ma ke ʻano he ʻenehana airtight i manaʻo hou ʻia e wehewehe ʻia penei.
(2) Me ka ruler, e kaha i ka laina ma ka ili o ka ili palaki no ka hoomaopopo ana i ke kulana o na apana FRP, he 2.5 knm ka mamao mawaena o na kaula.A laila, e kāʻei i ka lipine a puni nā wahi kaʻa kahi i pono ʻole ai ka FRP.
(3) Hoʻomaʻamaʻa maikaʻi ʻia ka ʻili o ke kaʻa me ke one, holoi ʻia me ka huluhulu waiʻona, a uhi ʻia me ka epoxy.A laila, e hoʻopaʻa lima i nā ʻili fiberglass ma luna o ka ʻili kaʻa a kaomi i waho i nā āpau i paʻa pono ka fiberglass i ka ʻili kaukau a pale i nā ʻōhū ea.ʻO ka hope, e kāpili i nā ʻāpana FRP ma luna o ka ʻili kaʻa mai luna a lalo, e like me nā kaha i hana ʻia me kahi lula.
(4) Ma hope o ka hapalua hola, e nānā inā ua kaʻawale ke kaʻa mai ka FRP.Inā paheʻe a paʻa paha ka FRP, pono e hoʻoponopono koke.Pono e ho'ōla ʻia nā mea hoʻohālike i hoʻoheheʻe ʻia no 7 mau lā e hōʻoia i ka ikaika hoʻōla.
(5) Ma hope o ka ho'ōla ʻana, e hoʻohana i ka pahi pono no ka wehe ʻana i ka lipine mai ka ʻili paʻa, a loaʻa i kahi kolamu semi-hermetic FRP.
Hōʻike ʻia nā hopena ma lalo o nā kaohi like ʻole ma ka fig.2. Hōʻike ka Figure 2a i kahi pahu CFRP i hoʻopaʻa paʻa ʻia, Hōʻike ka Figure 2b i kahi ʻāpana CFRP semi-generalized, Hōʻike ka Figure 2c i kahi pahu GFRP i hoʻopaʻa ʻia, a hōʻike ka Figure 2d i kahi CFRP semi-constrained.
Nā ʻano i hoʻopili ʻia: (a) CFRP paʻa piha;(b) ka pulupulu kalapona pani pani;(c) paʻa loa i loko o ke aniani aniani;(d) aniani aniani i hoʻopaʻa ʻia.
ʻEhā mau ʻāpana nui i hoʻolālā ʻia no ka noiʻi ʻana i ka hopena o nā kaohi FRP a me nā kaʻina erosion ma ka hana hoʻomalu erosion o nā cylinders.Hōʻike ka Papa 3 i ka helu o nā kolamu kolamu.ʻO nā laʻana no kēlā me kēia ʻāpana he ʻekolu mau laʻana kūlana like e mālama i ka ʻikepili.Ua kālailai ʻia ka mean o ʻekolu laʻana no nā hopena hoʻokolohua āpau ma kēia ʻatikala.
(1) Hoʻokaʻawale ʻia nā mea paʻa ea ma ke ʻano he carbon fiber a i ʻole fiberglass.Ua hoʻohālikelike ʻia ka hopena o nā ʻano fiber ʻelua i ka hoʻoikaika ʻana o ke kaʻa.
(2) Hoʻokaʻawale ʻia nā ʻano hana hoʻopaʻa kolamu i ʻekolu ʻano: palena piha, semi-limited a me ka palena ʻole.Ua hoʻohālikelike ʻia ke kūʻē ʻana o nā kolamu semi-enclosed me nā ʻano ʻano ʻē aʻe ʻelua.
(3) ʻO nā pōʻaiapili hoʻoheheʻe ʻia ʻo ia nā pōʻai maloʻo maloʻo a me ka solution sulfate, a ʻo ka helu o nā pōʻai maloʻo maloʻo he 0, 50 a me 100 mau manawa.Ua aʻo ʻia ka hopena o ka hoʻohui ʻia ʻana ma nā kolamu līlū i hoʻopaʻa ʻia e FRP.
(4) Ua māhele ʻia nā ʻāpana hoʻāʻo i ʻekolu pūʻulu.ʻO ka pūʻulu mua ka FRP wrapping a laila corrosion, ʻo ka hui ʻelua he corrosion ma mua a laila ʻōwili ʻia, a ʻo ke kolu o ka hui he corrosion mua a laila ʻōwili a laila corrosion.
Ke hoʻohana nei ke kaʻina hana hoʻokolohua i ka mīkini hoʻāʻo honua, kahi mīkini hoʻāʻo tensile, kahi ʻāpana pōʻaiapuni freeze-thaw (CDR-Z type), kahi microscope electron, kahi mika pH, kahi ana kānana, kahi mea hoʻoneʻe, kahi microscope electron SEM, a me kahi EDS energy spectrum analyzer i kēia haʻawina.ʻO ka laʻana he kolamu mūmū 10 knm ke kiʻekiʻe a he 20 knm ke anawaena.Ua hoʻōla ʻia ke koʻa i loko o 28 mau lā ma hope o ka ninini ʻana a me ka hoʻopaʻa ʻana, e like me ka hōʻike ʻana ma ke Kiʻi 3a.Hoʻopau ʻia nā laʻana a pau ma hope o ka hoʻolei ʻana a mālama ʻia no 28 mau lā ma 18-22°C a me 95% haʻahaʻa pili, a laila ua wahī ʻia kekahi mau laʻana me ka fiberglass.
Nā ʻano hoʻāʻo: (a) nā mea hana no ka mālama mau ʻana i ka mahana a me ka haʻahaʻa;(b) he mīkini pōʻai hoʻoheheʻe hau;(c) mīkini hoʻāʻo honua;(d) mea hōʻike pH;(e) ka nānā ʻana i nā microscopic.
Hoʻohana ka hoʻokolohua hoʻoheheʻe i ke ʻano hoʻoheheʻe uila e like me ka hōʻike ʻana ma ke Kiʻi 3b.Wahi a GB / T 50082-2009 "Durability Standards for Conventional Concrete", ua hoʻokomo piha ʻia nā mea hoʻohālike i loko o ka 10% sodium sulfate solution ma 15-20 ° C no 4 mau lā ma mua o ka hoʻoheheʻe ʻana a me ka thawing.Ma hope o kēlā, hoʻomaka ka hoʻouka ʻana o ka sulfate a hoʻopau i ka manawa like me ka pōʻaiapuni freeze-thaw.He 2 a 4 mau hola ka manawa hoʻoheheʻe hau, a ʻaʻole e emi iho ka manawa hoʻoheheʻe ma mua o 1/4 o ka manawa pōʻai.Pono e mālama ʻia ke anahana kumu ma loko o ka laulā mai (-18±2) a i (5±2) °C.ʻAʻole pono e ʻoi aku ma mua o ʻumi mau minuke ka hoʻololi ʻana mai ka hau a i ka defrosting.Ua hoʻohana ʻia ʻekolu mau laʻana like ʻole o kēlā me kēia ʻāpana no ke aʻo ʻana i ka pohō kaumaha a me ka hoʻololi ʻana o ka pH o ka hoʻonā ma luna o 25 mau pōʻai manuahi, e like me ka hōʻike ʻana ma ka Fig. 3d.Ma hope o kēlā me kēia 25 pōʻai maloʻo maloʻo, wehe ʻia nā laʻana a hoʻomaʻemaʻe ʻia nā ʻili ma mua o ka hoʻoholo ʻana i ko lākou kaumaha hou (Wd).Ua hoʻokō ʻia nā hoʻokolohua āpau i triplicate o nā laʻana, a ua hoʻohana ʻia nā kumukūʻai maʻamau e kūkākūkā i nā hopena hōʻike.Hoʻoholo ʻia nā ʻōkuhi no ka nalowale o ka nuipa a me ka ikaika o ka hāpana penei:
Ma ke kumu, ΔWd ka pohō kaumaha (%) o ka hāpana ma hope o kēlā me kēia 25 pōʻai hoʻoheheʻe ʻia, ʻo W0 ke kaumaha awelika o ka hāpana ʻākea ma mua o ka pōʻaiapuni manuahi-hoʻoheheʻe (kg), ʻo Wd ka awelika kaumaha.ke kaumaha o ka laʻana ma hope o 25 mau pōʻai maloʻo maloʻo (kg).
Hōʻike ʻia ka coefficient hoʻohaʻahaʻa ikaika o ka hāpana e Kd, a penei ka helu helu:
Ma ke kumu, ΔKd ka laiki o ka poho o ka ikaika (%) o ka la'ana ma hope o kela a me keia 50 kaapuni manuahi, f0 ka awelika o ka ikaika o ka la'ana pa'a ma mua o ke kaapuni manuahi (MPa), fd ka ikaika awelika o ka laʻana paʻa no 50 mau pōʻaiapuni manuahi (MPa).
Ma ka fig.Hōʻike ʻo 3c i kahi mīkini hoʻāʻo compressive no nā specimens.E like me ka "Standard for Test Methods for the Physical and Mechanical Properties of Concrete" (GBT50081-2019), ua wehewehe ʻia kahi ʻano hana no ka hoʻāʻo ʻana i nā kolamu koneki no ka ikaika compressive.ʻO 0.5 MPa/s ka nui o ka hoʻouka ʻana i ka hoʻāʻo ʻana, a hoʻohana ʻia ka hoʻouka ʻana a me ka hoʻouka ʻana i ka wā o ka hoʻāʻo.Ua hoʻopaʻa ʻia ka pilina hoʻoneʻe ukana no kēlā me kēia mea hoʻohālike i ka wā o ka hoʻāʻo mechanical.Ua hoʻopaʻa ʻia nā kānana kānana i nā ʻili o waho o ka ʻōpala a me nā ʻāpana FRP o nā specimens no ke ana ʻana i nā kaha axial a me ke ākea.Hoʻohana ʻia ka cell strain i ka hoʻāʻo mechanical e hoʻopaʻa i ka hoʻololi ʻana o ke kānana specimen i ka wā o ka hoʻāʻo ʻana.
ʻO kēlā me kēia 25 mau pōʻai maloʻo maloʻo, wehe ʻia kahi laʻana o ka solution freeze-thaw a waiho ʻia i loko o kahi pahu.Ma ka fig.Hōʻike ʻo 3d i kahi hōʻike pH o kahi hāpana hāpana i loko o kahi pahu.Hōʻike ʻia ma ke kiʻi 3d ka nānā ʻana microscopic o ka ʻili a me ka ʻāpana keʻa o ka hāpana ma lalo o nā kūlana hoʻoheheʻe hau.Ua ʻike ʻia ke kūlana o ka ʻili o nā laʻana like ʻole ma hope o 50 a me 100 mau pōʻai manuahi i ka solution sulfate ma lalo o kahi microscope.Hoʻohana ka microscope i ka hoʻonui 400x.I ka nānā ʻana i ka ʻili o ka hāpana, ʻike nui ʻia ka erosion o ka papa FRP a me ka ʻaoʻao o waho o ka ʻāpana.ʻO ka nānā ʻana i ka ʻāpana keʻa o ka hāpana koho maʻamau i nā kūlana erosion ma kahi mamao o 5, 10 a me 15 mm mai ka papa waho.Pono ka ho'āʻo hou ʻana i ka hoʻokumu ʻana i nā huahana sulfate a me nā pōʻai manuahi-thaw.No laila, ua nānā ʻia ka ʻili i hoʻololi ʻia o nā laʻana i koho ʻia me ka scanning electron microscope (SEM) i lako me ka ikehu dispersive spectrometer (EDS).
E nānā maka i ka ʻili o ka laʻana me kahi microscope electron a koho i ka hoʻonui 400X.He kiʻekiʻe loa ke kiʻekiʻe o ka pōʻino o ka ʻili i loko o ka pāpaʻa GRP semi-paʻa a hui ʻole ʻia ma lalo o nā pōʻai maloʻo maloʻo a me ka ʻike ʻana i nā sulfate, ʻoiai ʻo ka paʻa paʻa paʻa he mea ʻole.ʻO ka ʻāpana mua e pili ana i ka hiki ʻana mai o ka ʻānai ʻana o ke koki kahe manuahi e ka sodium sulfate a mai ka 0 a hiki i ka 100 mau pōʻai manuahi, e like me ka hōʻike ʻana ma ka Fig. 4a.ʻO nā laʻana paʻa ʻole me ka ʻike ʻole ʻana i ka hau he ʻili maʻemaʻe me nā hiʻohiʻona ʻike ʻole ʻia.Ma hope o 50 erosions, ʻili ʻia ka ʻāpana pulp ma ka ʻili, e hōʻike ana i ka ʻili keʻokeʻo o ka pulp.Ma hope o 100 erosions, ua hāʻule loa nā pūpū o nā hoʻonā i ka wā o ka nānā ʻana i ka ʻili ʻili.Ua hōʻike ʻia ka nānā ʻana i ka microscopic ua maʻalahi ka ʻili o ka 0 freeze-thaw eroded concrete a ʻo ka ʻili o ka ʻili a me ka pahū ma ka mokulele hoʻokahi.Ua ʻike ʻia ka ʻili like ʻole a ʻoʻoleʻa ma luna o ka ʻili līlū i hoʻopau ʻia e 50 mau pōʻai hau.Hiki ke wehewehe ʻia kēia ma ka ʻoiaʻiʻo o ka luku ʻia ʻana o kekahi o ka mortar a me kahi liʻiliʻi o nā keʻokeʻo keʻokeʻo keʻokeʻo e pili ana i ka ʻili, ʻo ia ka mea i haku ʻia i ka aggregate, mortar a me nā keʻokeʻo keʻokeʻo.Ma hope o 100 mau pōʻai manuahi, ua ʻike ʻia kahi ʻāpana nui o nā keʻokeʻo keʻokeʻo ma ka ʻili o ke kaʻa, ʻoiai ua hōʻike ʻia ka ʻāpana ʻeleʻele i waho.I kēia manawa, ʻike nui ʻia ka ʻili o ke kaʻa a me nā kristal keʻokeʻo.
Morphology o ka erosive freeze-thaw concrete kolamu: (a) unrestricted concrete column;(b) i hoʻopaʻa ʻia i ka ʻāpana kalapona i hoʻopaʻa ʻia;(c) GRP semi-paʻa paʻa;(d) hoʻopaʻa paʻa piha ʻia ʻo CFRP;(e) GRP sikika semi-paʻa paʻa.
ʻO ka ʻāpana ʻelua, ʻo ia ka ʻino o nā kolamu semi-hermetic CFRP a me GRP ma lalo o nā pōʻai maloʻo maloʻo a me ka ʻike ʻana i nā sulfate, e like me ka hōʻike ʻana ma Fig. 4b, c.Hōʻike ʻia ka nānā ʻana (1x hoʻonui) ua hoʻokumu ʻia kahi pauka keʻokeʻo ma luna o ka ʻili o ka papa fibrous, a hāʻule koke me ka piʻi ʻana o ka nui o nā pōʻai manuahi.Ua ʻoi aku ka manaʻo o ka ʻānai ʻana o ka ʻili o ka semi-hermetic FRP i ka piʻi ʻana o ka nui o nā pōʻai hau.ʻO ka ʻike ʻike ʻia o ka "bloating" (ʻo ka ʻaoʻao ākea o ka hopena o ke kolamu koneki ma ka ʻaoʻao o ka hāʻule ʻana).Eia nō naʻe, ua hoʻopilikia ʻia ke ʻano o ka ʻili ʻana e ka uhi ʻana o ka fiber carbon pili).Ma lalo o ka microscope, ʻike ʻia nā ʻili kalapona synthetic e like me nā kaula keʻokeʻo ma kahi ʻeleʻele ʻeleʻele ma 400x hoʻonui.Ma muli o ke ʻano poepoe o nā fiber a me ka ʻike ʻana i ka mālamalama ʻole, ʻike ʻia lākou ke keʻokeʻo, akā ʻeleʻele nā pūʻolo kalapona.He keʻokeʻo keʻokeʻo ka Fiberglass i ka wā mua, akā i ka hoʻopili ʻana me ka mea hoʻopili, lilo ia i akaka a ʻike maopopo ʻia ke ʻano o ke kaila i loko o ka fiberglass.He keʻokeʻo keʻokeʻo ka fiberglass a melemele ka mea paʻa.He māmā loa ka waihoʻoluʻu ʻelua, no laila e hūnā ke kala o ke kāpili i nā kaula fiberglass, e hāʻawi ana i ka nānā holoʻokoʻa i kahi ʻulaʻula melemele.Mālama ʻia ke kalapona a me ke aniani mai ka pōʻino e kahi resin epoxy waho.I ka hoʻonui ʻia ʻana o ka hoʻouka ʻana o ka hau hau, ua ʻike ʻia ka nui o nā hakahaka a me kekahi mau kristal keʻokeʻo ma ka ʻili.Ke piʻi aʻe nei ka pōʻai maloʻo sulfate, ʻoi aku ka lahilahi o ka mea hoʻopaʻa, nalowale ke kala melemele a ʻike ʻia nā fiber.
ʻO ke kolu o ka ʻāpana ʻo ia ka ʻinoʻino o ka CFRP a me GRP i hoʻopaʻa piha ʻia ma lalo o nā pōʻai maloʻo maloʻo a me ka ʻike ʻana i nā sulfate, e like me ka hōʻike ʻana ma ka Fig. 4d, e.Eia hou, ua like nā hualoaʻa i ʻike ʻia me nā ʻano ʻelua o ka ʻāpana i hoʻopaʻa ʻia o ke kolamu koneki.
E hoʻohālikelike i nā hanana i ʻike ʻia ma hope o ka hoʻohana ʻana i nā ʻano hana hoʻopaʻa ʻekolu i wehewehe ʻia ma luna.Paʻa mau nā ʻiʻo fibrous i loko o ka ʻiʻo FRP i hoʻopaʻa ʻia me ka piʻi ʻana o ka nui o nā pōʻai manuahi.Ma ka ʻaoʻao ʻē aʻe, ʻoi aku ka lahilahi o ke apo apo adhesive ma ka ʻili.Hoʻopili ka nui o nā resine epoxy me nā ion hydrogen ikaika i loko o ka ʻakika sulfuric apo hāmama a ʻaʻole hiki ke hana me nā sulfate28.No laila, hiki ke noʻonoʻo ʻia e hoʻololi nui ka erosion i nā waiwai o ka papa adhesive ma muli o nā pōʻai freeze-thaw, a laila hoʻololi i ka hopena hoʻoikaika o FRP.ʻO ka ʻili paʻa o FRP semi-hermetic concrete he ʻano erosion like ʻole me ka ʻili paʻa ʻole.ʻO kona papa FRP e pili ana i ka papa FRP o ka paʻa paʻa piha, a ʻaʻole maopopo ka pōʻino.Eia nō naʻe, i loko o ka pāpaʻi GRP semi-sealed, hiki mai nā māwae erosional nui ma kahi e hui ai nā ʻāpana fiber me ka ʻāpana i ʻike ʻia.ʻOi aku ke koʻikoʻi o ka ʻānai ʻana o nā ʻili kaʻa i ʻike ʻia i ka piʻi ʻana o ka nui o nā pōʻai hoʻoheheʻe.
Ua hōʻike ʻia nā ʻokoʻa koʻikoʻi o ka loko o ka paʻa paʻa piha, semi-paʻa, a me ka paʻa ʻole i ka wā i hoʻokau ʻia i nā pōʻai maloʻo a me ka ʻike ʻana i nā hopena sulfate.Ua ʻoki ʻia ka hāpana me ka transversely a ua nānā ʻia ka ʻāpana keʻa me ka microscope electron ma 400x magnification.Ma ka fig.Hōʻike ka 5 i nā kiʻi microscopic ma kahi lōʻihi o 5 mm, 10 mm a me 15 mm mai ka palena ma waena o ke kaʻa a me ka mortar.Ua ʻike ʻia i ka wā e hui pū ʻia ai ka solution sodium sulfate me ka freeze-thaw, e wāwahi ʻia ka pōʻino o ka ʻili mai ka ʻili a i loko.Ma muli o ka like o nā kūlana erosion o loko o CFRP a me GFRP-constrained concrete, ʻaʻole hoʻohālikelike kēia ʻāpana i nā mea waihona ʻelua.
ʻO ka nānā ʻana i ka microscopic o loko o ka ʻāpana kaʻa o ke kolamu: (a) kaupalena ʻia e ka fiberglass;(b) semi-paʻa me ka fiberglass;(c) palena ʻole.
Hōʻike ʻia ka hoʻoneʻe ʻana o ka FRP i hoʻopaʻa piha ʻia ma ka fig.5a.ʻIke ʻia nā māwae ma 5 mm, maʻalahi ka ʻili, ʻaʻohe crystallization.He laumania ka ʻili, ʻaʻohe kristal, 10 a 15 mm ka mānoanoa.Hōʻike ʻia ka hoʻohaʻahaʻa kūloko o FRP semi-hermetic concrete ma ka fig.5 B. ʻIke ʻia nā māwae a me nā keokeo keʻokeʻo ma 5mm a me 10mm, a maʻemaʻe ka ʻili ma 15mm.Hōʻike ka Figure 5c i nā ʻāpana o nā kolamu FRP paʻa kahi i loaʻa ai nā māwae ma 5, 10 a me 15 mm.ʻO kekahi mau aniani keʻokeʻo keʻokeʻo i loko o nā māwae ua lilo i mea kakaʻikahi i ka neʻe ʻana o nā māwae mai waho o ka pā a i loko.Ua hōʻike ʻia nā kolamu kaʻa pau ʻole i ka ʻinoʻino loa, a ukali ʻia e nā kolamu FRP semi-constrained.He liʻiliʻi ka hopena o ka sodium sulfate i loko o nā mea hoʻohālike FRP i hoʻopaʻa piha ʻia ma mua o 100 mau pōʻaiapuni manuahi.Hōʻike kēia ʻo ke kumu nui o ka ʻai ʻia ʻana o ka ʻōpala FRP i hoʻopaʻa piha ʻia e pili ana i ka hoʻoheheʻe ʻana i ka hau i kekahi manawa.Ma ka nānā ʻana i ka ʻāpana keʻa, ua maʻalahi ka ʻāpana ma mua o ka maloʻo ʻana a me ka hoʻoheheʻe ʻana a me ka ʻole o nā aggregates.I ka maloʻo ʻana a me ka hoʻoheheʻe ʻana o ke kaʻa, ʻike ʻia nā māwae, ʻoiaʻiʻo nō hoʻi no ka hōʻuluʻulu ʻana, a ua uhi paʻa ʻia nā kristal granular keʻokeʻo me nā māwae.Ua hōʻike ʻia nā haʻawina27 i ka wā e hoʻokomo ʻia ai ke kaʻa i loko o kahi solution sodium sulfate, e komo ka sodium sulfate i loko o ka ʻeke, e hoʻoheheʻe kekahi o ia mau mea e like me nā kristal sodium sulfate, a e hana kekahi me ka sima.ʻO nā kristal sodium sulfate a me nā huahana hopena e like me nā granula keʻokeʻo.
Hoʻopau loa ʻo FRP i nā māwae kaʻa i ka ʻili ʻana, akā paʻa ka ʻāpana me ka ʻole crystallization.Ma ka ʻaoʻao ʻē aʻe, ua hoʻomohala nā ʻāpana ʻāpana semi-pani a me ka palena ʻole o ka FRP i nā māwae kūloko a me ka crystallization ma lalo o ka hoʻoneʻe conjugated.E like me ka wehewehe ʻana o ke kiʻi a me nā haʻawina mua29, ua māhele ʻia ke kaʻina hana hoʻoneʻe ʻana o ke kaʻina FRP paʻa ʻole a me ka semi-restricted i ʻelua mau pae.Hoʻopili ʻia ka pae mua o ka māhā ʻana me ka hoʻonui a me ka ʻoki ʻana i ka wā hau.Ke komo ka sulphate i loko o ka koneki a ʻike ʻia, hoʻopiha ka sulphate pili i nā māwae i hana ʻia e ka emi ʻana mai ka hoʻoheheʻe ʻana a me ka hydration reactions.No laila, loaʻa i ka sulfate kahi hopena pale kūikawā ma ke kaʻa i ka wā mua a hiki ke hoʻomaikaʻi i nā ʻano mechanical o ka ʻuala i kekahi ʻano.Ke hoʻomau nei ka lua o ka hoʻouka ʻana i ka sulfate, e komo ana i nā māwae a i ʻole nā waha a me ka hana ʻana me ka sima e hana i ka alum.ʻO ka hopena, ulu ka māwae i ka nui a pōʻino.I loko o kēia manawa, ʻo ka hoʻonui ʻana a me ka hoʻokaʻawale ʻana e pili ana i ka hau a me ka hoʻoheheʻe ʻana e hoʻonui i ka pōʻino o loko o ka pahu, e hopena i ka emi ʻana o ka hiki ke amo.
Ma ka fig.Hōʻike ka 6 i ka hoʻololi ʻana o ka pH o nā hoʻonā impregnation koneki no ʻekolu mau ala palena i nānā ʻia ma hope o 0, 25, 50, 75, a me 100 nā pōʻai manuahi.Ua hōʻike ʻia ka piʻi wikiwiki loa o ka pH mai ka 0 a hiki i ka 25 mau pōʻaiapuni manuahi FRP.Ua hoʻonui ʻia ko lākou mau pH mai 7.5 a 11.5 a me 11.4.I ka piʻi ʻana o ka nui o nā pōʻai manuahi, ua emi iki ka piʻi ʻana o ka pH ma hope o 25-100 mau pōʻai manuahi.Ua hoʻonui ʻia ko lākou mau pH mai 11.5 a me 11.4 a i 12.4 a me 11.84.No ka mea ua uhi ʻia ka ʻāpana FRP paʻa paʻa piha i ka papa FRP, paʻakikī ke komo ʻana i ka solution sodium sulfate.I ka manawa like, paʻakikī ke komo ʻana o ka sima i loko o nā hopena o waho.No laila, ua piʻi mālie ka pH mai 7.5 a i 8.0 ma waena o 0 a me 100 mau pōʻaiapuni freeze-thaw.Hoʻopili ʻia ke kumu o ka hoʻololi ʻana i ka pH penei.Hoʻohui ʻia ka silicate i loko o ke koneki me nā iona hydrogen i loko o ka wai e hana ai i ka ʻakika silicic, a ʻo ke koena OH- e hoʻonui i ka pH o ka hopena saturated.Ua ʻoi aku ka nui o ka hoʻololi ʻana o ka pH ma waena o 0-25 mau pōʻaiapuni freeze-thaw a ʻoi aku ka liʻiliʻi ma waena o 25-100 mau pōʻaiapuni freeze-thaw30.Eia nō naʻe, ua ʻike ʻia ma ʻaneʻi ua hoʻomau ka piʻi ʻana o ka pH ma hope o 25-100 mau pōʻaiapuni freeze-thaw.Hiki ke wehewehe ʻia kēia ma ka ʻoiaʻiʻo o ka sodium sulfate e hoʻopili i ke kemika me ka loko o ka koneki, e hoʻololi i ka pH o ka hopena.Hōʻike ka ʻike ʻana o ka haku mele ʻana i ka hana ʻana o ke koneki me ka sodium sulfate ma ke ʻano aʻe.
Hōʻike nā formula (3) a me (4) i ka sodium sulfate a me ka calcium hydroxide i loko o ka sima ma ke ʻano he gypsum (calcium sulfate), a ʻo ka calcium sulfate e hana hou aku me ka calcium metaaluminate i loko o ka sima e hana ai i nā kristal alum.Hoʻopili ʻia ka pane (4) me ka hoʻokumu ʻana i ka OH- kumu, e alakaʻi ana i ka piʻi ʻana o ka pH.Eia kekahi, no ka mea hiki ke hoʻohuli ʻia kēia hopena, piʻi ka pH i kekahi manawa a loli mālie.
Ma ka fig.Hōʻike ka 7a i ka pohō kaumaha o ka pāpaʻa GRP i hoʻopaʻa ʻia, semi-paʻa, a i hoʻopaʻa ʻia i ka wā o nā pōʻai maloʻo maloʻo i loko o ka solution sulfate.ʻO ka hoʻololi ʻoi loa o ka pohō nui ʻana ʻo ia ka lāʻau paʻa ʻole.Ua nalowale ke kaʻa paʻa ʻole ʻia ma kahi o 3.2% o kona nui ma hope o 50 hoʻouka ʻana i ka hau hau a ma kahi o 3.85% ma hope o ka hoʻouka ʻana o 100 freeze-thaw.Hōʻike nā hopena i ka emi ʻana o ka hopena o ka erosion conjugated i ka maikaʻi o ke kahe kahe ʻokoʻa i ka piʻi ʻana o ka nui o nā pōʻai manuahi.Eia nō naʻe, i ka nānā ʻana i ka ʻili o ka hāpana, ua ʻike ʻia ua ʻoi aku ka nui o ka nalowale o ka mortar ma hope o 100 mau pōʻai manuahi ma mua o 50 mau pōʻai manuahi.Hoʻohui ʻia me nā haʻawina ma ka pauku mua, hiki ke manaʻo ʻia ʻo ke komo ʻana o ka sulfates i loko o ka ʻiʻo e alakaʻi i ka emi ʻana o ka pohō nui.I kēia manawa, ʻo ka alum a me ka gypsum i hoʻokumu ʻia i loko ka hopena i ka emi ʻana o ke kaumaha, e like me ka wānana e nā hoʻohālikelike kemika (3) a me (4).
Hoʻololi paona: (a) pilina ma waena o ka hoʻololi paona a me ka helu o nā pōʻai maloʻo maloʻo;(b) ka pilina ma waena o ka hoʻololi nuipa a me ka waiwai pH.
ʻO ka hoʻololi o ke kaumaha o ka FRP semi-hermetic concrete e emi mua ana a laila e hoʻonui.Ma hope o 50 mau pōʻaiapuni freeze-thaw, ʻo ka nui o ka nalowale o ka semi-hermetic fiberglass concrete ma kahi o 1.3%.ʻO ke kaumaha ma hope o 100 cycles he 0.8%.No laila, hiki ke hoʻoholo ʻia e komo ka sodium sulfate i loko o ke kahe manuahi.Eia kekahi, ua hōʻike ʻia ka nānā ʻana i ka ʻili o ka ʻāpana hoʻāʻo e hiki i nā ʻāpana fiber ke pale aku i ka ʻili ʻana i ka mortar ma kahi ākea, a laila e hōʻemi ana i ka pohō kaumaha.
ʻOkoʻa ka hoʻololi ʻana o ka nui o ka lilo ʻana o ka pahu FRP i hoʻopaʻa ʻia mai nā mea mua ʻelua.ʻAʻole nalowale ka Mass, akā hoʻohui.Ma hope o 50 frost-thaw erosions, piʻi ka nui ma kahi o 0.08%.Ma hope o 100 mau manawa, ua hoʻonui ʻia kona nuipa ma kahi o 0.428%.Ma muli o ka ninini ʻia ʻana o ke koʻi, ʻaʻole e hemo ka mortar ma luna o ka ʻili o ka ʻili a ʻaʻole hiki ke hopena i ka nalowale o ka maikaʻi.Ma ka ʻaoʻao ʻē aʻe, ʻo ke komo ʻana o ka wai a me nā sulfate mai ka ʻili kiʻekiʻe o ka ʻike i loko o ka ʻāpana haʻahaʻa haʻahaʻa e hoʻomaikaʻi ai i ka maikaʻi o ka ʻili.
Ua hana mua ʻia kekahi mau haʻawina e pili ana i ka pilina ma waena o ka pH a me ka nui o ka lilo ʻana i ka pahu paʻa FRP ma lalo o nā kūlana erosive.ʻO ka hapa nui o ka noiʻi e kūkākūkā nui i ka pilina ma waena o ka pohō nui, modulus elastic a me ka nalowale ikaika.Ma ka fig.Hōʻike ka 7b i ka pilina ma waena o ka pH koneki a me ka poho nui ma lalo o ʻekolu mau kaohi.Manaʻo ʻia kahi kŘkohu wānana e wānana i ka nalo nuipaʻa paʻa me ka hoʻohana ʻana i ʻekolu mau ʻano paʻa ma nā koina pH like ʻole.E like me ka mea i ʻike ʻia ma ke Kiʻi 7b, kiʻekiʻe ka coefficient o Pearson, e hōʻike ana aia nō ka pilina ma waena o ka pH a me ka poho nui.ʻO nā kumukūʻai r-squared no ka paʻa ʻole, semi-palena, a me ka paʻa piha ʻana he 0.86, 0.75, a me 0.96.Hōʻike kēia i ka hoʻololi ʻana o ka pH a me ka pohō kaumaha o ke kaila i hoʻopaʻa ʻia piha i ka laina ma lalo o nā kūlana sulfate a me ka hau hau.I loko o ka paʻa paʻa ʻole a me ka semi-hermetic FRP concrete, piʻi mālie ka pH i ka wā e hana ai ka sima me ka wai wai.ʻO ka hopena, ua hoʻopau mālie ʻia ka ʻili o ke kaʻa, kahi e hiki ai i ke kaumaha ʻole.Ma ka ʻaoʻao ʻē aʻe, hoʻololi liʻiliʻi ka pH o ke kaila paʻa piha no ka mea e hoʻolohi ka papa FRP i ka hopena kemika o ka sima me ka wai.No laila, no ka paʻa paʻa paʻa, ʻaʻohe ʻike ʻia o ka ʻili o ka ʻili, akā e loaʻa ke kaumaha ma muli o ka saturation ma muli o ka absorption o nā hopena sulfate.
Ma ka fig.Hōʻike ka 8 i nā hopena o kahi scan SEM o nā laʻana i kālai ʻia me ka sodium sulfate freeze-thaw.Ua nānā ʻia ka microscopy electron i nā laʻana i hōʻiliʻili ʻia mai nā poloka i lawe ʻia mai ka papa o waho o nā kolamu palaki.He kiʻi kiʻi microscope electron kiʻi kiʻi 8a o ke kiʻi i hoʻopaʻa ʻole ʻia ma mua o ka hū ʻana.Hoʻomaopopo ʻia he nui nā puka ma ka ʻili o ka hāpana, kahi e hoʻopilikia ai i ka ikaika o ke kolamu kaʻa ponoʻī ma mua o ka hau.Ma ka fig.Hōʻike ʻo 8b i kahi kiʻi microscope electron o kahi laʻana paʻa paʻa FRP i hoʻopaʻa ʻia ma hope o 100 mau pōʻai manuahi.Hiki ke ʻike ʻia nā māwae i loko o ka hāpana ma muli o ka hau a me ka hoʻolulu.Eia naʻe, maʻalahi ka ʻili a ʻaʻohe kristal ma luna.No laila, ʻike ʻia nā māwae i hoʻopiha ʻole ʻia.Ma ka fig.Hōʻike ʻo 8c i kahi laʻana o ka semi-hermetic GRP kaila ma hope o 100 mau pōʻaiapili hau.Ua akaka ka nui o ka māwae a me ka hana ʻana o nā māwae ma waena o nā māwae.Hoʻopili kekahi o kēia mau ʻāpana iā lākou iho i nā māwae.Hōʻike ʻia kahi hōʻike SEM o kahi laʻana o kahi kolamu kaʻa ʻole i hoʻopaʻa ʻia ma ke Kiʻi 8d, kahi hanana i kūlike me ka semi-restriction.No ka hoʻomaʻamaʻa hou ʻana i ke ʻano o nā ʻāpana, ua hoʻonui ʻia a nānā ʻia nā ʻāpana i loko o nā māwae me ka hoʻohana ʻana i ka spectroscopy EDS.Hele mai nā ʻāpana i ʻekolu ʻano like ʻole.E like me ka nānā ʻana o ka ikehu spectrum, ʻo ke ʻano mua, e like me ka mea i hōʻike ʻia ma ke Kiʻi 9a, he aniani poloka maʻamau, i haku ʻia me O, S, Ca a me nā mea ʻē aʻe.Ma ka hoʻohui ʻana i nā kumu mua (3) a me (4), hiki ke hoʻoholo ʻia ʻo ka mea nui o ka mea he gypsum (calcium sulfate).Hōʻike ʻia ka lua ma ke Kiʻi 9b;e like me ka ikehu spectrum analysis, he acicular non-directional object, a o kona mau mea nui he O, Al, S a me Ca.Hōʻike ʻia nā ʻōkuhi hui ʻana he alum ka mea nui.ʻO ke kolu o ka poloka i hōʻike ʻia ma ka Fig. 9c, he poloka like ʻole ia, i hoʻoholo ʻia e ka nānā ʻana i ka spectrum ikehu, ʻo ka hapa nui o nā ʻāpana O, Na a me S. Ua ʻike ʻia ʻo ia ka nui o nā kristal sodium sulfate.Ua hōʻike ʻia ka microscopy electron scanning ua hoʻopiha ʻia ka hapa nui o nā puka i nā kristal sodium sulfate, e like me ka hōʻike ʻana ma ke Kiʻi 9c, me nā mea liʻiliʻi o ka gypsum a me ka alum.
Electron microscopic kiʻi o nā laʻana ma mua a ma hope o ka ʻino ʻana: (a) wehe ʻia ke koʻa ma mua o ka ʻino ʻana;(b) ma hope o ka ʻino ʻana, ua hoʻopaʻa ʻia ka fiberglass;(c) ma hope o ka ʻino ʻana o ka GRP semi-paʻa paʻa;(d) ma hope o ka ʻino ʻia ʻana o ke kaila hāmama.
Hiki iā mākou ke unuhi i nā hopena hope.ʻO nā kiʻi microscope electron o nā laʻana ʻekolu he 1k × āpau a ʻike ʻia nā māwae a me nā huahana erosion a nānā ʻia i nā kiʻi.Loaʻa nā māwae laula loa a loaʻa i nā kīʻaha he nui.ʻOi aku ka haʻahaʻa o ka FRP semi-pressure ma mua o ke kaomi ʻole ma ke ʻano o ka laula māwae a me ka helu ʻāpana.Loa'a ka laula māwae li'ili'i loa o ka pāpa'i FRP i ho'opa'a piha 'ia a 'a'ohe mea ma hope o ka hili 'ana o ka hau.ʻO kēia mau mea a pau e hōʻike ana i ka paʻa piha ʻana o FRP ka mea maʻalahi loa i ka hū ʻana mai ka hau a me ka hoʻoheheʻe.ʻO nā kaʻina hana kemika i loko o nā kolamu semi-paʻa a wehe ʻia ʻo FRP e alakaʻi i ka hoʻokumu ʻana o ka alum a me ka gypsum, a ʻo ke komo ʻana o ka sulfate e pili ana i ka porosity.ʻOiai ʻo nā pōʻaiapuni freeze-thaw ke kumu nui o ka haki ʻana o ke kō, nā sulfate a me kā lākou huahana e hoʻopiha i kekahi o nā māwae a me nā pores ma kahi mua.Eia nō naʻe, i ka piʻi ʻana o ka nui a me ka manawa o ka erosion, hoʻomau ka hoʻonui ʻia o nā māwae a piʻi ka nui o ka alum i hana ʻia, e hopena i nā māwae extrusion.ʻO ka hope loa, ʻo ka hoʻoheheʻe ʻana i ka hau a me ka sulfate e hōʻemi i ka ikaika o ke kolamu.